AZ91C T4

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where AZ91C T4 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

1.9 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

48 GPa at 20 °C

Show Magnesium materials with Elastic modulus of 48 GPa at 20 °C

Elongation

A

8.1 % at 20 °C

Show Magnesium materials with Elongation of 8.1 % at 20 °C

Poisson's ratio

ν

0.28 [-] at 20 °C

Show Magnesium materials with Poisson's ratio of 0.28 [-] at 20 °C

Typical for Magnesium

Tensile strength

Rm

270 MPa at 20 °C

Show Magnesium materials with Tensile strength of 270 MPa at 20 °C

Yield strength

YS

85 MPa at 20 °C

Show Magnesium materials with Yield strength of 85 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.6E-5 1/K at 20 °C

Melting point

Tm

470 °C

Specific heat capacity

cp

990 J/(kg·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Mg

88.6 - 91.4 %

Al

8.1 - 9.3 %

Zn

0.4 - 1 %

Mn

0.13 - 0.35 %

Cu

0 - 0.1 %

More

This material data has been provided by MakeItFrom.com.