AZ91E T6

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

1.9 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

44 GPa at 23 °C

Show Magnesium materials with Elastic modulus of 44 GPa at 23 °C

Elongation

A

4 % at 23 °C

Show Magnesium materials with Elongation of 4 % at 23 °C

Poisson's ratio

ν

0.29 [-] at 23 °C

Show Magnesium materials with Poisson's ratio of 0.29 [-] at 23 °C

Typical for Magnesium

Shear modulus

G

45 GPa at 23 °C

Show Magnesium materials with Shear modulus of 45 GPa at 23 °C

Typical for Magnesium

Tensile strength

Rm

250 MPa at 23 °C

Show Magnesium materials with Tensile strength of 250 MPa at 23 °C

Yield strength

YS

130 MPa at 23 °C

Show Magnesium materials with Yield strength of 130 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.7E-5 1/K at 23 °C

Melting point

Tm

500 °C

Specific heat capacity

cp

1000 J/(kg·K) at 23 °C

Thermal conductivity

λ

84 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Mg

88.8 - 91.3 %

Al

8.1 - 9.3 %

Zn

0.4 - 1 %

Mn

0.17 - 0.35 %

Cu

0 - 0.02 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.