UNS N06230 Cast

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where UNS N06230 Cast falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

9.9 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

210 GPa at 23 °C

Show Nickel Chromium Molybdenum Alloy materials with Elastic modulus of 210 GPa at 23 °C

Elongation

A

38 % at 23 °C

Show Nickel Chromium Molybdenum Alloy materials with Elongation of 38 % at 23 °C

Tensile strength

Rm

620 MPa at 23 °C

Show Nickel Chromium Molybdenum Alloy materials with Tensile strength of 620 MPa at 23 °C

Yield strength

YS

330 MPa at 23 °C

Show Nickel Chromium Molybdenum Alloy materials with Yield strength of 330 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 1/K at 23 °C

Melting point

Tm

1300 °C

Specific heat capacity

cp

400 J/(kg·K) at 23 °C

Thermal conductivity

λ

9 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Ni

47.5 - 65.2 %

Cr

20 - 24 %

W

13 - 15 %

Mo

1 - 3 %

Mn

0.3 - 1 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.