Density
ρ7.3 g/cm³ at 23 °C
Coefficient of thermal expansion
α2.1E-5 1/K at 23 °C
Melting point
Tm240 °C
Specific heat capacity
cp220 J/(kg·K) at 23 °C
Thermal conductivity
λ52 - 74 W/(m·K) at 23 °C
Typical for Tin
Element
Weight %
Comment
90 - 93 %
5 - 7.5 %
1.5 - 3 %
0 - 0.05 %
0 - 0.02 %