See where ASTM Grade 9 Cold Worked And Stress Relieved falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ4.5 g/cm³ at 20 °C
Coefficient of thermal expansion
α9.1E-6 1/K at 20 °C
Melting point
Tm1668 °C
Typical for Titanium
Specific heat capacity
cp490 J/(kg·K) at 20 °C
Thermal conductivity
λ8.1 W/(m·K) at 20 °C
Electrical conductivity
σel4.23E+7 S/m at 20 °C
Element
Weight %
Comment
92.6 - 95.5 %
2.5 - 3.5 %
2 - 3 %
0 - 0.08 %
0 - 0.02 %
This material data has been provided by MakeItFrom.com.