ZA-27 Die Cast

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

5 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

78 GPa at 23 °C

Show Zinc Aluminium materials with Elastic modulus of 78 GPa at 23 °C

Elongation

A

2 % at 23 °C

Show Zinc Aluminium materials with Elongation of 2 % at 23 °C

Poisson's ratio

ν

0.3 [-] at 23 °C

Show Zinc Aluminium materials with Poisson's ratio of 0.3 [-] at 23 °C

Typical for Zinc Aluminium

Tensile strength

Rm

430 MPa at 23 °C

Show Zinc Aluminium materials with Tensile strength of 430 MPa at 23 °C

Yield strength

YS

370 MPa at 23 °C

Show Zinc Aluminium materials with Yield strength of 370 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.6E-5 1/K at 23 °C

Melting point

Tm

380 °C

Specific heat capacity

cp

530 J/(kg·K) at 23 °C

Thermal conductivity

λ

130 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Zn

69.3 - 73 %

Al

25 - 28 %

Cu

2 - 2.5 %

Mg

0.01 - 0.02 %

Cd

0 - 6E-3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.