ZA-8 Die Cast

Want to keep this datasheet? Save it now in your required format

Ashby charts

See where ZA-8 Die Cast falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

6.3 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

86 GPa at 23 °C

Show Zinc Aluminium materials with Elastic modulus of 86 GPa at 23 °C

Elongation

A

8 % at 23 °C

Show Zinc Aluminium materials with Elongation of 8 % at 23 °C

Poisson's ratio

ν

0.3 [-] at 23 °C

Show Zinc Aluminium materials with Poisson's ratio of 0.3 [-] at 23 °C

Typical for Zinc Aluminium

Tensile strength

Rm

370 MPa at 23 °C

Show Zinc Aluminium materials with Tensile strength of 370 MPa at 23 °C

Yield strength

YS

290 MPa at 23 °C

Show Zinc Aluminium materials with Yield strength of 290 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.3E-5 1/K at 23 °C

Melting point

Tm

380 °C

Specific heat capacity

cp

440 J/(kg·K) at 23 °C

Thermal conductivity

λ

120 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Zn

89.7 - 91.2 %

Al

8 - 8.8 %

Cu

0.8 - 1.3 %

Mg

0.02 - 0.03 %

Cd

0 - 6E-3 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.