See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ11 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.2E-5 1/K at 23 °C
Melting point
Tm1550 °C
Specific heat capacity
cp240 J/(kg·K) at 23 °C
Thermal conductivity
λ60 - 76 W/(m·K) at 23 °C
Typical for Palladium
Element
Weight %
Comment
99.8 - 100 %
0 - 0.2 %
This material data has been provided by MakeItFrom.com.