General
Property | Value | Temperature |
---|---|---|
Density | 11 g/cm³ Show Material materials with Density of 11 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 110 GPa Show Material materials with Elastic modulus of 110 GPa at 23.0 °C | 23.0 °C | |
Elongation | 1.2 % Show Material materials with Elongation of 1.2 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.39 [-] Show Material materials with Poisson's ratio of 0.39 [-] at 23.0 °C | 23.0 °C | Typical for Palladium |
Shear modulus | 42 GPa Show Material materials with Shear modulus of 42 GPa at 23.0 °C | 23.0 °C | Typical for Palladium |
Tensile strength | 360 MPa Show Material materials with Tensile strength of 360 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 1550 °C Show Material materials with Melting point of 1550 °C | ||
Specific heat capacity | 240 J/(kg·K) Show Material materials with Specific heat capacity of 240 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 60 - 76 W/(m·K) Show Material materials with Thermal conductivity of 60 - 76 W/(m·K) at 23.0 °C | 23.0 °C | Typical for Palladium |
Chemical properties
Property | ||
---|---|---|
Other | 0 - 0.2 % | |
Palladium | 99.8 - 100 % |