Silver (Ag) Half-Hard

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

10 g/cm³

Show Material materials with Density of 10 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

83 GPa

Show Material materials with Elastic modulus of 83 GPa

Elongation

23.0 °C

4.6 %

Show Material materials with Elongation of 4.6 %

Poisson's ratio

23.0 °C

0.37 [-]

Show Material materials with Poisson's ratio of 0.37 [-]

Typical for Silver

Shear modulus

23.0 °C

30 GPa

Show Material materials with Shear modulus of 30 GPa

Typical for Silver

Tensile strength

23.0 °C

260 MPa

Show Material materials with Tensile strength of 260 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2E-5 1/K

Melting point

962 °C

Show Material materials with Melting point of 962 °C

Typical for Silver

Specific heat capacity

23.0 °C

240 J/(kg·K)

Show Material materials with Specific heat capacity of 240 J/(kg·K)

Thermal conductivity

23.0 °C

417 - 428 W/(m·K)

Show Material materials with Thermal conductivity of 417 - 428 W/(m·K)

Typical for Silver

Chemical properties

PropertyValue

Other

0 - 0.1 %

Show Material materials with Other of 0 - 0.1 %

Silver

99.9 - 100 %

Show Material materials with Silver of 99.9 - 100 %