Monel 400 Hot Worked

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

9 g/cm³

Show Material materials with Density of 9 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperature

Elastic modulus

180 GPa

Show Material materials with Elastic modulus of 180 GPa at 23.0 °C

23.0 °C

Elongation

37 %

Show Material materials with Elongation of 37 % at 23.0 °C

23.0 °C

Tensile strength

600 MPa

Show Material materials with Tensile strength of 600 MPa at 23.0 °C

23.0 °C

Yield strength

260 MPa

Show Material materials with Yield strength of 260 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K at 23.0 °C

23.0 °C

Melting point

1300 °C

Show Material materials with Melting point of 1300 °C

Specific heat capacity

430 J/(kg·K)

Show Material materials with Specific heat capacity of 430 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

23 W/(m·K)

Show Material materials with Thermal conductivity of 23 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Carbon

0 - 0.3 %

Copper

28 - 34 %

Iron

0 - 2.5 %

Manganese

0 - 2 %

Nickel

63 - 72 %

Silicon

0 - 0.5 %

Sulfur

0 - 0.024 %