Monel K-500 Hot Worked

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperature

Elastic modulus

180 GPa

Show Material materials with Elastic modulus of 180 GPa at 23.0 °C

23.0 °C

Elongation

30 %

Show Material materials with Elongation of 30 % at 23.0 °C

23.0 °C

Tensile strength

850 MPa

Show Material materials with Tensile strength of 850 MPa at 23.0 °C

23.0 °C

Yield strength

500 MPa

Show Material materials with Yield strength of 500 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.4E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 1/K at 23.0 °C

23.0 °C

Melting point

1320 °C

Show Material materials with Melting point of 1320 °C

Specific heat capacity

420 J/(kg·K)

Show Material materials with Specific heat capacity of 420 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

18 W/(m·K)

Show Material materials with Thermal conductivity of 18 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Aluminium

2.3 - 3.2 %

Carbon

0 - 0.18 %

Copper

27 - 33 %

Iron

0 - 2 %

Manganese

0 - 1.5 %

Nickel

63 - 70.4 %

Silicon

0 - 0.5 %

Sulfur

0 - 0.01 %

Titanium

0.35 - 0.85 %