Description

Nature Alu High Purity Aluminum 4N (99.99% Al) is produced from a segregation process, also known as fractional crystallization. Because hydroelectricity is used as the main energy source, the process generates much less carbone dioxide than other aluminum purification processes. Nature Alu is proud to produce High Purity Aluminum with the lowest carbon footprint in the industry.

This material data has been provided by Nature Alu.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueComment

Aluminium

99.99 %

Show Supplier Material materials with Aluminium of 99.99 %

Chromium

0.0007 %

Show Supplier Material materials with Chromium of 0.0007 %

Copper

1e-05 %

Show Supplier Material materials with Copper of 1e-05 %

Less than

Gallium

0.002 %

Show Supplier Material materials with Gallium of 0.002 %

Iron

0.001 %

Show Supplier Material materials with Iron of 0.001 %

Magnesium

0.0001 %

Show Supplier Material materials with Magnesium of 0.0001 %

Manganese

0.001 %

Show Supplier Material materials with Manganese of 0.001 %

Nickel

0.0002 %

Show Supplier Material materials with Nickel of 0.0002 %

Other

0.001 %

Show Supplier Material materials with Other of 0.001 %

Silicon

0.003 %

Show Supplier Material materials with Silicon of 0.003 %

Titanium

0.0001 %

Show Supplier Material materials with Titanium of 0.0001 %

Vanadium

0.001 %

Show Supplier Material materials with Vanadium of 0.001 %

Zinc

0.0008 %

Show Supplier Material materials with Zinc of 0.0008 %

Technological properties

Property
Application areas

High Purity Aluminum / Capacitor foil / Current collectors / Additive manufacturing / 3D printing / Specilaty alloys / Powder / Sapphire / Battery (Li-ion, Al-Air)

Delivery condtion

Available delivery forms:

  • Sow of approximatively 600kg
  • Ingots of 10kg

  • Other

    Listed chemical properties represent typical values obtained by Nature Alu. Purity adjustments can be made to meet customer needs on a case-by-case basis. The comment "Less than" means that the value is under the OES limit of detection.