Akestra™ 100 is an amorphous copolyester with sparkling glass-like clarity suitable for food packaging containers, sheets and films as well as in durables. It has outstanding features in heat resistance, chemical resistance and hydrolytic stability. Akestra™ has excellent processing properties, is easy to process in standard PET equipment and can be used in most polymer processes like extrusion casting and coating, injection molding. The high melt strength also enables good processability in film blowing and blow molding.

Akestra™ 100 is compatible with PET and can be coextruded with PET and used in thermoforming of cups for hotfill as a sustainable replacement for PS. Akestra™ may be used in food contact application and complies both with FDA and EU regulations for direct food contact.

This material data has been provided by Perstorp.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 %

Show Supplier Material materials with Elongation of 200 %

ASTM D638

Flexural modulus

20.0 °C

2.5 GPa

Show Supplier Material materials with Flexural modulus of 2.5 GPa

ASTM D790

Flexural yield strength

20.0 °C

90 MPa

Show Supplier Material materials with Flexural yield strength of 90 MPa

ASTM D790

Impact strength, Izod notched, ASTM

20.0 °C

25 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 25 J/m

ASTM D256

Thermal

PropertyValueComment

Glass transition temperature

100 °C

Show Supplier Material materials with Glass transition temperature of 100 °C

ASTM D7426

Heat deflection temperature, 0.45 MPa

86 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 86 °C

ASTM D648

Optical

PropertyValueComment

Haze

1 %

Show Supplier Material materials with Haze of 1 %

ASTM D1003

Luminous transmittance

90 [-]

Show Supplier Material materials with Luminous transmittance of 90 [-]

ASTM D1003

Technological properties

Property
Application areas

Food packaging containers, blow molding, sheets and films as well as in durables injection molding articles.

Compliance

Akestra™ and/or its monomers are approved as food contact material in Europe (EFSA) and USA (FDA). Akestra™ complies with RoHS. All raw materials are REACH registered. A document of compliance is available on request with details about its regulatory and compliances.

Processing methods

Desiccant dryer and/or vented extrusion equipment.

  • Drying Time: 8-10 hours
  • Max. Drying Temp.: 80 ˚C
  • Dew point: < -29 ˚C
  • Processing melt temp. 220-270˚C
  • Mold Temperature. 20-60˚C