Glass Fiber Reinforced Grade, 33% glass fiber reinforced

Meet the requirements of higher stiffness, strength and heat distortion temperature

This material data has been provided by RebornPlas Composites Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.38 g/cm³

Show Supplier Material materials with Density of 1.38 g/cm³

ASTM D792

Water absorption, equilibrium

23.0 °C

0.3 %

Show Supplier Material materials with Water absorption, equilibrium of 0.3 %

max., ASTM D4442

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

5 %

Show Supplier Material materials with Elongation of 5 %

max., ASTM D638

Flexural modulus

23.0 °C

8.2 GPa

Show Supplier Material materials with Flexural modulus of 8.2 GPa

ASTM D790

Flexural strength

23.0 °C

240 MPa

Show Supplier Material materials with Flexural strength of 240 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

120 [-]

Show Supplier Material materials with Hardness, Rockwell R of 120 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

90 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m

ASTM D256

Tensile strength

23.0 °C

150 MPa

Show Supplier Material materials with Tensile strength of 150 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

33 %

Show Supplier Material materials with Ash content of 33 %

ASTM D482

Heat deflection temperature, 1.80 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 - 0.6 %

Show Supplier Material materials with Shrinkage of 0.2 - 0.6 %

ASTM D955

Technological properties

Property
Application areas

Sports equipment, Hand tool, Bicycle brake parts, Office desk & chair, Home appliance parts, Motor housing, Hairdryer nozzle, Electrical and Pneumatic Hand Tools-Hot melt glue gun housing, Office Chair Armrest

Color

White

Fillers

45% Glass Fiber