Polyamide 6 (PA6) A3000TBKA3

Alternative and trade names
PA6-I
Want to keep this datasheet? Save it now in your required format

Description

Ultra Impact Modified Grade, Low Temperature Impact Resistance

Excellent stiffness, strength and low warpage, suitable for electroplating processing characteristics

This material data has been provided by RebornPlas Composites Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

ASTM D792

Water absorption, equilibrium

23.0 °C

0.3 %

Show Supplier Material materials with Water absorption, equilibrium of 0.3 %

max., ASTM D4442

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ASTM D638

Flexural modulus

23.0 °C

1.75 GPa

Show Supplier Material materials with Flexural modulus of 1.75 GPa

ASTM D790

Flexural strength

23.0 °C

70 MPa

Show Supplier Material materials with Flexural strength of 70 MPa

ASTM D790

Hardness, Shore D

23.0 °C

72 [-]

Show Supplier Material materials with Hardness, Shore D of 72 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

-30.0 °C

160 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m

min., ASTM D256

23.0 °C

800 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 800 J/m

min., ASTM D256

Tensile strength

23.0 °C

43 MPa

Show Supplier Material materials with Tensile strength of 43 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

50 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

20 g/10min

Show Supplier Material materials with Melt mass-flow rate of 20 g/10min

min., ASTM D1238

Shrinkage

23.0 °C

1.6 - 2 %

Show Supplier Material materials with Shrinkage of 1.6 - 2 %

ASTM D955

Technological properties

Property
Application areas

Sports equipment, Plug, Fan blades, Plastic screw, Gear, Bicycle brake disc, Nut, Suitcase wheel, Office Chairs caster

Color

Black