Polyamide 66 (PA66) B2040BK

Want to keep this datasheet? Save it now in your required format

Description

General Grade

High stiffness and strength, heat resistance and hydrolysis resistance

This material data has been provided by RebornPlas Composites Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.14 g/cm³

Show Supplier Material materials with Density of 1.14 g/cm³

ASTM D792

Water absorption, equilibrium

23.0 °C

0.3 %

Show Supplier Material materials with Water absorption, equilibrium of 0.3 %

max., ASTM D4442

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

2 %

Show Supplier Material materials with Elongation of 2 %

min., ASTM D638

Flexural modulus

23.0 °C

2.8 GPa

Show Supplier Material materials with Flexural modulus of 2.8 GPa

ASTM D790

Flexural strength

23.0 °C

120 MPa

Show Supplier Material materials with Flexural strength of 120 MPa

ASTM D790

Hardness, Shore D

23.0 °C

80 [-]

Show Supplier Material materials with Hardness, Shore D of 80 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

50 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m

ASTM D256

Tensile strength

23.0 °C

68 MPa

Show Supplier Material materials with Tensile strength of 68 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

2 %

Show Supplier Material materials with Ash content of 2 %

max., ASTM D482

Heat deflection temperature, 1.80 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

70 - 250 g/10min

Show Supplier Material materials with Melt mass-flow rate of 70 - 250 g/10min

ASTM D1238

Shrinkage

23.0 °C

1.2 - 1.6 %

Show Supplier Material materials with Shrinkage of 1.2 - 1.6 %

ASTM D955

Technological properties

Property
Application areas

Washer, Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing , Sports equipment, Gear, Sporting goods-Glasses temples Automobiles parts

Color

Black