Polyamide 66 (PA66) B1000GV25NC

Alternative and trade names
PA6-GF25
Want to keep this datasheet? Save it now in your required format

Description

Glass Fiber Reinforced/Flame Retardant Grade, 25% glass fiber reinforced

High flame resistance, high strength and dimensional stability

This material data has been provided by RebornPlas Composites Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.53 g/cm³

Show Supplier Material materials with Density of 1.53 g/cm³

ASTM D792

Water absorption, equilibrium

23.0 °C

0.3 %

Show Supplier Material materials with Water absorption, equilibrium of 0.3 %

max., ASTM D4442

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

5 %

Show Supplier Material materials with Elongation of 5 %

min., ASTM D638

Flexural modulus

23.0 °C

7.84 GPa

Show Supplier Material materials with Flexural modulus of 7.84 GPa

ASTM D790

Flexural strength

23.0 °C

210 MPa

Show Supplier Material materials with Flexural strength of 210 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

115 [-]

Show Supplier Material materials with Hardness, Rockwell R of 115 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

90 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m

ASTM D256

Tensile strength

23.0 °C

135 MPa

Show Supplier Material materials with Tensile strength of 135 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

25 %

Show Supplier Material materials with Ash content of 25 %

ASTM D482

Heat deflection temperature, 1.80 MPa

230 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 230 °C

ASTM D648

Flammability

UL94 V0

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.4 - 0.6 %

Show Supplier Material materials with Shrinkage of 0.4 - 0.6 %

ASTM D955

Technological properties

Property
Application areas

Headlight cover. Connector, Terminal block, Plug. Electrical switch housing, Breaker, Motor parts. Cooling Fan, Power tools, Machine tool motor housing.

Color

Natural

Fillers

25% Glass Fiber