Copolyamide 6/66 (PA6/66) C2201GT30BKE1

Alternative and trade names
PA66+PA6-GF30
Want to keep this datasheet? Save it now in your required format

Description

Glass Fiber Reinforced/Impact Modified, Impact resistant 30% glass fiber reinforced

Excellent ultra high toughness and low temperature impact resistance

This material data has been provided by RebornPlas Composites Co., Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.33 g/cm³

Show Supplier Material materials with Density of 1.33 g/cm³

ASTM D792

Water absorption, equilibrium

23.0 °C

0.3 %

Show Supplier Material materials with Water absorption, equilibrium of 0.3 %

max., ASTM D4442

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

5 %

Show Supplier Material materials with Elongation of 5 %

max., ASTM D638

Flexural modulus

23.0 °C

6.86 GPa

Show Supplier Material materials with Flexural modulus of 6.86 GPa

ASTM D790

Flexural strength

23.0 °C

205 MPa

Show Supplier Material materials with Flexural strength of 205 MPa

ASTM D790

Hardness, Rockwell R

23.0 °C

120 [-]

Show Supplier Material materials with Hardness, Rockwell R of 120 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

160 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m

ASTM D256

Tensile strength

23.0 °C

130 MPa

Show Supplier Material materials with Tensile strength of 130 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

30 %

Show Supplier Material materials with Ash content of 30 %

ASTM D482

Heat deflection temperature, 1.80 MPa

245 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 245 °C

ASTM D648

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 - 0.8 %

Show Supplier Material materials with Shrinkage of 0.3 - 0.8 %

ASTM D955

Technological properties

Property
Application areas

Automobiles-Rearview mirror Rotation Axes, Medical Equipment-Wheelchair Fork

Color

Black

Fillers

30% Glass Fiber