Description

Nylon 6, glass fiber reinforced product with antioxidant and lubricant

This material data has been provided by Henan Shenma Warwick Plastic Co., Ltd..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.25 g/cm³

Show Supplier Material materials with Density of 1.25 g/cm³

ISO1183

Water absorption

23.0 °C

1.25 %

Show Supplier Material materials with Water absorption of 1.25 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

6.5 %

Show Supplier Material materials with Elongation of 6.5 %

ISO527

Flexural modulus

23.0 °C

4.5 GPa

Show Supplier Material materials with Flexural modulus of 4.5 GPa

ISO178

Flexural strength

23.0 °C

175 MPa

Show Supplier Material materials with Flexural strength of 175 MPa

ISO178

Impact strength, Charpy notched

23.0 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO179

Impact strength, Charpy unnotched

23.0 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

ISO179

Tensile strength

23.0 °C

125 MPa

Show Supplier Material materials with Tensile strength of 125 MPa

ISO527

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ISO 75/A

Melting point

225 - 230 °C

Show Supplier Material materials with Melting point of 225 - 230 °C

ISO3146

Flammability

HB UL94

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

GB/T 1408

Volume resistivity

23.0 °C

1.00E+17 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm

GB/T1410

Technological properties

Property
Application areas

Automotive industry, mechanical shields, blades, gears, power tools, etc.

Fillers

18% Glass Fiber