Nylon 66, glass fiber reinforced and toughened product with antioxidant

This material data has been provided by Henan Shenma Warwick Plastic Co., Ltd..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.37 g/cm³

Show Supplier Material materials with Density of 1.37 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

7 %

Show Supplier Material materials with Elongation of 7 %

ISO527

Flexural modulus

23.0 °C

7.5 GPa

Show Supplier Material materials with Flexural modulus of 7.5 GPa

ISO178

Flexural strength

23.0 °C

250 MPa

Show Supplier Material materials with Flexural strength of 250 MPa

ISO178

Impact strength, Charpy notched

23.0 °C

18 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m²

ISO179

Impact strength, Charpy unnotched

23.0 °C

95 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

ISO179

Tensile strength

23.0 °C

175 MPa

Show Supplier Material materials with Tensile strength of 175 MPa

ISO527

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

245 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 245 °C

ISO 75/A

Melting point

260 - 270 °C

Show Supplier Material materials with Melting point of 260 - 270 °C

ISO3146

Flammability

HB UL94

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

22 kV/mm

Show Supplier Material materials with Dielectric strength of 22 kV/mm

GB/T 1408

Volume resistivity

23.0 °C

1.00E+17 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm

GB/T1410

Technological properties

Property
Application areas

For high-speed railway

Fillers

32% Glass Fiber