PP PPG-20

Alternative and trade names
PP-GF20, PPG-20
Want to keep this datasheet? Save it now in your required format

Description

Glass fiber reinforced PP compounding resin with antioxidant and lubricant

This material data has been provided by Henan Shenma Warwick Plastic Co., Ltd..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.05 g/cm³

Show Supplier Material materials with Density of 1.05 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

ISO527

Flexural modulus

23.0 °C

4.3 GPa

Show Supplier Material materials with Flexural modulus of 4.3 GPa

ISO178

Flexural strength

23.0 °C

100 MPa

Show Supplier Material materials with Flexural strength of 100 MPa

ISO178

Impact strength, Charpy unnotched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

ISO179

Tensile strength

23.0 °C

70 MPa

Show Supplier Material materials with Tensile strength of 70 MPa

ISO527

Technological properties

Property
Application areas

Automotive industry, consumer goods, etc.

Fillers

20% Glass Fiber