PBT P27GF-230

Alternative and trade names
PBT-GF30, P27GF-230
Want to keep this datasheet? Save it now in your required format

Description

Glass fiber reinforced PBT compounding resin with flame retardant and antioxidant

This material data has been provided by Henan Shenma Warwick Plastic Co., Ltd..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.42 g/cm³

Show Supplier Material materials with Density of 1.42 g/cm³

ISO1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

5 %

Show Supplier Material materials with Elongation of 5 %

ISO527

Flexural strength

23.0 °C

65 MPa

Show Supplier Material materials with Flexural strength of 65 MPa

ISO178

Impact strength, Charpy notched

23.0 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

ISO179

Impact strength, Charpy unnotched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

ISO179

Tensile strength

23.0 °C

120 MPa

Show Supplier Material materials with Tensile strength of 120 MPa

ISO527

Thermal

PropertyValueComment

Melting point

205 - 215 °C

Show Supplier Material materials with Melting point of 205 - 215 °C

ISO3146

Electrical

PropertyTemperatureValueComment

Volume resistivity

23.0 °C

1.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm

GB/T1410

Technological properties

Property
Application areas

Electronics, home appliances, automotive industry, etc.

Fillers

30% Glass Fiber