AISI 1020 Cold Rolled

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Shanghai Metal Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

200 GPa

Show Supplier Material materials with Elastic modulus of 200 GPa

Elongation

23.0 °C

26 %

Show Supplier Material materials with Elongation of 26 %

Tensile strength

23.0 °C

355 - 500 MPa

Show Supplier Material materials with Tensile strength of 355 - 500 MPa

Yield strength

23.0 °C

355 - 490 MPa

Show Supplier Material materials with Yield strength of 355 - 490 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.19E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.19E-5 1/K

Specific heat capacity

23.0 °C

486 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 486 J/(kg·K)

Thermal conductivity

23.0 °C

51.9 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 51.9 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.59E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.59E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.18 - 0.23 %

Show Supplier Material materials with Carbon of 0.18 - 0.23 %

Copper

0.2 %

Show Supplier Material materials with Copper of 0.2 %

Iron

Balance

Manganese

0.3 - 0.6 %

Show Supplier Material materials with Manganese of 0.3 - 0.6 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Sulfur

0.05 %

Show Supplier Material materials with Sulfur of 0.05 %