St 37-2 Hot Rolled

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Shanghai Metal Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Supplier Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

200 - 210 GPa

Show Supplier Material materials with Elastic modulus of 200 - 210 GPa

Elongation

23.0 °C

17 %

Show Supplier Material materials with Elongation of 17 %

Tensile strength

23.0 °C

340 - 510 MPa

Show Supplier Material materials with Tensile strength of 340 - 510 MPa

Yield strength

23.0 °C

225 MPa

Show Supplier Material materials with Yield strength of 225 MPa

Thermal

PropertyTemperatureValue

Specific heat capacity

23.0 °C

461 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 461 J/(kg·K)

Thermal conductivity

23.0 °C

54 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 54 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

1.5E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.5E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.2 %

Show Supplier Material materials with Carbon of 0.2 %

Iron

Balance

Manganese

1.25 %

Show Supplier Material materials with Manganese of 1.25 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.12 %

Show Supplier Material materials with Silicon of 0.12 %

Sulfur

0.035 %

Show Supplier Material materials with Sulfur of 0.035 %