Inconel 625

Want to keep this datasheet? Save it now in your required format

Description

Inconel 625 is a nonmagnetic, corrosion and oxidation resistant, nickel-base alloy. It has high strength and toughness in the temperature range cryogenic to 1093°C which is derived largely from the solid solution effects of the refractory metals, columbium and molybdenum, in a nickel-chromium matrix.

Equivalent Materials

This material data has been provided by Shanghai Metal Corporation.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Supplier Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

30 %

Show Supplier Material materials with Elongation of 30 %

Tensile strength

23.0 °C

760 MPa

Show Supplier Material materials with Tensile strength of 760 MPa

Yield strength

23.0 °C

345 MPa

Show Supplier Material materials with Yield strength of 345 MPa

Chemical properties

PropertyValueComment

Aluminium

0.4 %

Show Supplier Material materials with Aluminium of 0.4 %

Carbon

0.1 %

Show Supplier Material materials with Carbon of 0.1 %

Chromium

20 - 23 %

Show Supplier Material materials with Chromium of 20 - 23 %

Copper

0.5 %

Show Supplier Material materials with Copper of 0.5 %

Iron

5 %

Show Supplier Material materials with Iron of 5 %

Manganese

0.5 %

Show Supplier Material materials with Manganese of 0.5 %

Molybdenum

8 - 10 %

Show Supplier Material materials with Molybdenum of 8 - 10 %

Nickel

58 %

Show Supplier Material materials with Nickel of 58 %

Niobium

3.15 - 4.15 %

Show Supplier Material materials with Niobium of 3.15 - 4.15 %

plus Hydrogen

Phosphorus

0.02 %

Show Supplier Material materials with Phosphorus of 0.02 %

Silicon

0.5 %

Show Supplier Material materials with Silicon of 0.5 %

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

Titanium

0.4 %

Show Supplier Material materials with Titanium of 0.4 %

Technological properties

Property
Application areas

1. The organic chemical process parts contain chloride, especially in the use of acid chloride catalyst. 2. Absorption tower, re-heater, gas import board, fan, blender, fair water fin, flue and so on for using in flue gas desulfurization system. 3. The equipment and parts in the use of acidic gas environments. 4. Sulfur acid cooling