Description

Duplex UNS S31803 is the most common duplex grade in the market with high mechanical strength. It is widely used in Oil & Gas Industry, hydro power, pressure vessels, pulp & Equipment for the Paper Industry, Paper Industry, structural components and chemical tankers. The alloy is not intended to be used at temperatures above 300°C due to embrittlement.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

32 - 250 mm

Show Supplier Material materials with Diameter of 32 - 250 mm

Mechanical

PropertyTemperatureValue

Charpy impact energy, V-notch

-46.0 °C

45 J

Show Supplier Material materials with Charpy impact energy, V-notch of 45 J

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Hardness, Brinell

23.0 °C

270 [-]

Show Supplier Material materials with Hardness, Brinell of 270 [-]

Tensile strength

23.0 °C

650 - 880 MPa

Show Supplier Material materials with Tensile strength of 650 - 880 MPa

Yield strength Rp0.2

23.0 °C

450 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 450 MPa

Chemical properties

PropertyValue

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

Chromium

21 - 23 %

Show Supplier Material materials with Chromium of 21 - 23 %

Iron

Balance

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

Molybdenum

2.5 - 3.5 %

Show Supplier Material materials with Molybdenum of 2.5 - 3.5 %

Nickel

4.5 - 6.5 %

Show Supplier Material materials with Nickel of 4.5 - 6.5 %

Nitrogen

0.1 - 0.22 %

Show Supplier Material materials with Nitrogen of 0.1 - 0.22 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

Technological properties

Property
Application areas

It is widely used in Oil & Gas Industry, hydro power, pressure vessels, pulp & Equipment for the Paper Industry, structural components and chemical tankers.

Corrosion properties

High resistance to stress corrosion cracking in halide containing environments, High resistance to pitting and crevice corrosion, High resistance to general corrosion, High resistance to erosion corrosion and corrosion fatigue. PREN ≥ 34

Heat Treatment

Solution annealing at 1020 – 1100°C followed by water quenching.

Welding

Very good