UNS S32760 CR Plate

Alternative and trade names
EN 1.4501, UNS S32760, ASTM A182 Grade F55
.XLSX
.PDF
Save

Description

Super Duplex UNS S32760 is among the most common super duplex grade in the market. UNS S32760 is a duplex stainless steel especially designed for service in aggressive chloride-containing environments and has additions of W and Cu compared to UNS S32750. It has very good resistance to localized corrosion and stress corrosion cracking in combination with high mechanical strength.

Related Standards

Properties

Dimension

Length l

3000 - 6000 mm

Thickness t

1.5 - 50 mm

Width w

1500 - 2000 mm

Mechanical

Elongation A

25 % at 20 °C

Impact strength, Charpy notched Ivnot

45 kJ/m² at -46 °C

Tensile strength Rm

750 - 1000 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

550 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cr

24 - 26 %

Ni

6 - 8 %

Mo

3 - 4 %

Mn

1 %

Si

1 %

More

Technological properties

Processing history

Solution annealing at 1100°C followed by water quenching.

Welding

Very good.

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.