Dimension
Property | Value |
---|---|
Diameter | 3 - 650 mm Show Supplier Material materials with Diameter of 3 - 650 mm |
Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -195.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Elongation | 23.0 °C | 30 - 40 % Show Supplier Material materials with Elongation of 30 - 40 % |
Hardness, Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Hardness, Brinell of 215 [-] |
Tensile strength | 23.0 °C | 515 - 690 MPa Show Supplier Material materials with Tensile strength of 515 - 690 MPa |
Yield strength Rp0.2 | 23.0 °C | 205 MPa Show Supplier Material materials with Yield strength Rp0.2 of 205 MPa |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Supplier Material materials with Carbon of 0.03 % |
Chromium | 16 - 18 % Show Supplier Material materials with Chromium of 16 - 18 % |
Iron | Balance |
Manganese | 2 % Show Supplier Material materials with Manganese of 2 % |
Molybdenum | 2 - 3 % Show Supplier Material materials with Molybdenum of 2 - 3 % |
Nickel | 10 - 14 % Show Supplier Material materials with Nickel of 10 - 14 % |
Nitrogen | 0.01 % Show Supplier Material materials with Nitrogen of 0.01 % |
Phosphorus | 0.45 % Show Supplier Material materials with Phosphorus of 0.45 % |
Silicon | 0.75 % Show Supplier Material materials with Silicon of 0.75 % |
Sulfur | 0.03 % Show Supplier Material materials with Sulfur of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | The austenitic stainless steel AISI 316L shows good acid resistance. Material AISI 316L is used in the chemical industry, apparatus engineering, sewage plants and piping industry. | |
Heat Treatment | Solution annealed and quenched in air or water. | |
Welding | Very good |