TITANIUM GRADE 2 Plate

Alternative and trade names
TITANIUM GRADE 2
Want to keep this datasheet? Save it now in your required format

Description

Titanium Grade 2 is a pure alpha titanium. With moderate strength and excellent corrosion resistance and formability, Grade 2 titanium represents the most widely used form of titanium. Compared to the other grades of commercially pure titanium, Grade 2 titanium is slightly weaker than Grade 3, but stronger than Grade 1 and equally resistant to corrosion. Titanium grade 2 is non-magnetic. These properties account for Grade 2 titanium’s versatility in regard to its applications.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Length

3000 mm

Show Supplier Material materials with Length of 3000 mm

Thickness

2 - 30 mm

Show Supplier Material materials with Thickness of 2 - 30 mm

Width

1500 mm

Show Supplier Material materials with Width of 1500 mm

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

20 %

Show Supplier Material materials with Elongation of 20 %

Hardness, Rockwell B

23.0 °C

160 [-]

Show Supplier Material materials with Hardness, Rockwell B of 160 [-]

Tensile strength

23.0 °C

345 MPa

Show Supplier Material materials with Tensile strength of 345 MPa

Yield strength Rp0.2

23.0 °C

276 - 448 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 276 - 448 MPa

Chemical properties

PropertyValue

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

Hydrogen

0.02 %

Show Supplier Material materials with Hydrogen of 0.02 %

Iron

0.3 %

Show Supplier Material materials with Iron of 0.3 %

Nitrogen

0.03 %

Show Supplier Material materials with Nitrogen of 0.03 %

Oxygen

0.25 %

Show Supplier Material materials with Oxygen of 0.25 %

Titanium

Balance

Technological properties

Property
Application areas

Grade 2 titanium is also used to manufacture heat exchangers and cryogenic vessels. In seawater, Grade 2 is fully resistant to corrosion at temperatures up to 300°C.

Corrosion properties

It is highly resistant to chemical environments including oxidizing media, alkaline media, organic acids and compounds, aqueous salt solutions and hot gases. Its corrosion resistance holds up in liquid metals, nitric acid, mildly reducing acids and wet chlorine or bromine gas.