Description

AISI 4130 is a low alloy C-steel containing chromium and molybdenum as strengthening agents. It has low carbon content, and hence it can be welded easily. It is supplied as round bar commonly in the hardened and tempered condition with a hardness of 18-22 HRc.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

130 - 304.8 mm

Show Supplier Material materials with Diameter of 130 - 304.8 mm

Mechanical

PropertyTemperatureValue

Charpy impact energy, V-notch

-32.0 °C

42 J

Show Supplier Material materials with Charpy impact energy, V-notch of 42 J

Elongation

23.0 °C

17 - 18 %

Show Supplier Material materials with Elongation of 17 - 18 %

Hardness, Rockwell C

23.0 °C

22 [-]

Show Supplier Material materials with Hardness, Rockwell C of 22 [-]

Tensile strength

23.0 °C

585 - 655 MPa

Show Supplier Material materials with Tensile strength of 585 - 655 MPa

Yield strength Rp0.2

23.0 °C

414 - 517 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 414 - 517 MPa

Chemical properties

PropertyValue

Carbon

0.28 - 0.33 %

Show Supplier Material materials with Carbon of 0.28 - 0.33 %

Chromium

0.8 - 1.1 %

Show Supplier Material materials with Chromium of 0.8 - 1.1 %

Iron

Balance

Manganese

0.4 - 0.6 %

Show Supplier Material materials with Manganese of 0.4 - 0.6 %

Molybdenum

0.15 - 0.25 %

Show Supplier Material materials with Molybdenum of 0.15 - 0.25 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

Silicon

0.15 - 0.35 %

Show Supplier Material materials with Silicon of 0.15 - 0.35 %

Sulfur

0.035 %

Show Supplier Material materials with Sulfur of 0.035 %

Technological properties

Property
Application areas

AISI 4130 is a low alloyed hardened and tempered steel used for Oil and gas drilling and production equipment – wellhead and Christmas tree equipment.

Heat Treatment

Hardened at 860°C followed by water quenching. Tempering at min. 650°C, cooled in air.

Welding

Good.