ALLOY SUPER 13CR (S41426) Hardened and Tempered Bar

Alternative and trade names
ALLOY SUPER 13CR, UNS S41426
Want to keep this datasheet? Save it now in your required format

Description

X2CrNiMoV13-5-2 (1.4415) is developed from the standard 13Cr grade and offer enhanced mechanical properties and corrosion resistance. The low carbon improves weldability whilst maintaining the martensitic microstructure.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

76.2 - 254 mm

Show Supplier Material materials with Diameter of 76.2 - 254 mm

Mechanical

PropertyValueTemperature

Charpy impact energy, V-notch

60 J

Show Supplier Material materials with Charpy impact energy, V-notch of 60 J at -10.0 °C

-10.0 °C

Elongation

20 %

Show Supplier Material materials with Elongation of 20 % at 23.0 °C

23.0 °C

Hardness, Rockwell C

27 [-]

Show Supplier Material materials with Hardness, Rockwell C of 27 [-] at 23.0 °C

23.0 °C

Tensile strength

724 MPa

Show Supplier Material materials with Tensile strength of 724 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

655 - 724 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 655 - 724 MPa at 23.0 °C

23.0 °C

Chemical properties

Property

Carbon

0.03 %

Chromium

11.5 - 13.5 %

Iron

Balance

Manganese

1 %

Molybdenum

1.5 - 2.5 %

Nickel

4.5 - 6 %

Phosphorus

0.02 %

Silicon

0.5 %

Sulfur

5E-3 %

Titanium

0.01 - 0.5 %

Vanadium

0.5 %

Technological properties

Property
Application areas

Commonly used in the same area as AISI 4130, 4140 and 4145 but often in environment, which have a high content of sulfur.

Heat Treatment

Hardened and tempered

Welding

Moderate