S165M QT760 Bar

Alternative and trade names
S165M, ALLOY 1.4418, S165M, 2387
Want to keep this datasheet? Save it now in your required format

Description

S165M is a high strength low carbon martensitic/ austenitic stainless steel. It combines high strength, good fatigue resistance with good weldability, properties which are maintained after welding. Two minimum tensile levels are often used; QT760 and QT900. QT900 is mostly used by the industry.

Related Standards

Equivalent Materials

This material data has been provided by Sverdrup Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

10 - 410 mm

Show Supplier Material materials with Diameter of 10 - 410 mm

Mechanical

PropertyTemperatureValue

Charpy impact energy, V-notch

23.0 °C

80 J

Show Supplier Material materials with Charpy impact energy, V-notch of 80 J

Elongation

23.0 °C

16 %

Show Supplier Material materials with Elongation of 16 %

Hardness, Brinell

23.0 °C

280 - 340 [-]

Show Supplier Material materials with Hardness, Brinell of 280 - 340 [-]

Tensile strength

23.0 °C

760 - 960 MPa

Show Supplier Material materials with Tensile strength of 760 - 960 MPa

Yield strength Rp0.2

23.0 °C

550 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 550 MPa

Chemical properties

PropertyValue

Carbon

0.06 %

Show Supplier Material materials with Carbon of 0.06 %

Chromium

15 - 17 %

Show Supplier Material materials with Chromium of 15 - 17 %

Iron

Balance

Manganese

0.6 - 1.5 %

Show Supplier Material materials with Manganese of 0.6 - 1.5 %

Molybdenum

0.8 - 1.5 %

Show Supplier Material materials with Molybdenum of 0.8 - 1.5 %

Nickel

4 - 6 %

Show Supplier Material materials with Nickel of 4 - 6 %

Nitrogen

0.02 %

Show Supplier Material materials with Nitrogen of 0.02 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

Silicon

0.3 - 0.7 %

Show Supplier Material materials with Silicon of 0.3 - 0.7 %

Sulfur

0.005 - 0.03 %

Show Supplier Material materials with Sulfur of 0.005 - 0.03 %

Technological properties

Property
Application areas

The alloy has been designed to resist erosion corrosion or cavitation experienced in hydraulic applications. General areas for applications: Shafts, propellers, spindles, bolts, etc.

Corrosion properties

S165M is designed for application in slightly corrosive environment. Corrosion resistance is at the level of AISI 304L in most environments, however insensitive to intergranular corrosion.

Heat Treatment

QT760

Welding

Good, the low carbon martensite with the finely dispersed residual austenite yields an excellent HAZ toughness in the as welded condition. Preheating to 100°C – 200°C is suggested for very thick section or when the stress concentration after cooling require it.