SUS 310S Stainless Steel

Want to keep this datasheet? Save it now in your required format

Description

TJC Steel can supply ASTM A240/ A240M 310S (UNS S31008) Pressure Vessel Stainless Steel Plate/Coil/Strip, mainly used in the field which has a high request for corrosion resistance.

Equivalent Materials

This material data has been provided by TJC Iron & Steel.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.98 g/cm³

Show Supplier Material materials with Density of 7.98 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

Tensile strength

23.0 °C

515 MPa

Show Supplier Material materials with Tensile strength of 515 MPa

Yield strength

23.0 °C

205 MPa

Show Supplier Material materials with Yield strength of 205 MPa

Chemical properties

PropertyValue

Carbon

0.08 %

Show Supplier Material materials with Carbon of 0.08 %

Chromium

24 - 26 %

Show Supplier Material materials with Chromium of 24 - 26 %

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

Nickel

19 - 22 %

Show Supplier Material materials with Nickel of 19 - 22 %

Phosphorus

0.05 %

Show Supplier Material materials with Phosphorus of 0.05 %

Silicon

1.5 %

Show Supplier Material materials with Silicon of 1.5 %

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

Technological properties

Property
Application areas

Pressure Vessel& Anti-Corrosion Building