General
Property | Value |
---|---|
Bio-based content | 98.0 % Show Supplier Material materials with Bio-based content of 98.0 % |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 13.5 GPa Show Supplier Material materials with Elastic modulus of 13.5 GPa | ISO 527 |
Elongation | 1.0 Show Supplier Material materials with Elongation of 1.0 | ISO 527 |
Flexural modulus | 13.5 GPa Show Supplier Material materials with Flexural modulus of 13.5 GPa | ISO 178 |
Impact strength, Charpy notched | 10.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10.0 kJ/m² | ISO 179 |
Impact strength, Charpy unnotched | 44.0 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 44.0 kJ/m² | |
Tensile strength | 150.0 MPa Show Supplier Material materials with Tensile strength of 150.0 MPa | ISO 527 |
Thermal
Property | Value | Pressure | Comment |
---|---|---|---|
Heat deflection temperature | 198.0 °C Show Supplier Material materials with Heat deflection temperature of 198.0 °C | 1.8 MPa | ISO 75-1/A |
209.0 °C Show Supplier Material materials with Heat deflection temperature of 209.0 °C | 0.45 MPa | ISO 75-1/B | |
Melting point | 220.0 °C Show Supplier Material materials with Melting point of 220.0 °C | DSC |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber | |
Other | NOTICE REGARDING USE RESTRICTIONS: Unless specifically agreed to in writing, Total Corbion PLA will not knowingly market any product into any of the following commercial or developmental applications: | |
Processing methods | The compounded product should be dried to <400ppm before injection molding. Precautions should be taken to avoid moisture absorption of the dried granulate during processing, for example while sitting in the hopper of the injection molding machine. In general, injection molding conditions should be selected to avoid high stresses and high (back) pressures on the material in order to limit length reduction of the glass fibers. It is recommended to select an injection molding machine with a low ratio of barrel volume / show weight to avoid degradation in the barrel. A barrel volume of maximum 5 times the shot weight is recommended. The achievable cycle time for automatic operation depends on a number of machine, mold and product properties. As the product needs time to crystallize into full stereocomplex PLA, the crystallization time in the mold typically at 120°C is the rate limiting step. Although automatic operation will also run using lower mold cooling temperatures, this is not recommended because this will result in products with reduced thermal and dimensional stability. Typical settings, may require optimization: |