Show me around

Polystyrene (PS) for Extrusion

Alternative and trade names
HI-PS Black
Want to keep this datasheet? Save it now in your required format

Description

Recycled polystyrene granulate for extrusion. In addition to the standard reclaimed polymer portfolio, WELA Plast offers individually optimized customer specific formulations, especially when it comes to customized product colors and property profiles.

Ashby charts

See where Polystyrene (PS) for Extrusion falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Ash content

cash

3 % at 625 °C

DIN EN ISO 3451-1:1997

Density

ρ

1.06 g/cm³ at 20 °C

DIN EN ISO 1183-1

Melt mass-flow rate

MFR

7.5 g/10min at 220 °C

DIN EN ISO 1133-1 (220°C/5kg)

Mechanical

Impact strength, Charpy notched

Ivnot

Eq. DIN 179-1

Technological properties

Color

Black

Processing Tag

Do you need more data regarding this material?

This material data has been provided by Wela Plast.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.