Description

Recycled high density polyethylene granulate for extrusion. In addition to the standard reclaimed polymer portfolio, WELA Plast offers individually optimized customer specific formulations, especially when it comes to customized product colors and property profiles.

Properties

General

Ash content

cash

0.03 - 3 % at 625 °C

DIN EN ISO 3451-1:1997

Density

ρ

0.94 - 0.97 g/cm³ at 20 °C

DIN EN ISO 1183-1

Melt mass-flow rate

MFR

0.02 - 0.5 g/10min at 190 °C

DIN EN ISO 1133-1 (190°C/2.16kg)

Mechanical

Technological properties

Color

Natural, white, black, blue, yellow, jazz

Modifications

Processing Tag

Do you need more data regarding this material?

This material data has been provided by Wela Plast.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.