General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.03 g/cm³ Show Supplier Material materials with Density of 1.03 g/cm³ | ASTM D792 |
Water absorption | 23.0 °C | 1.7 % Show Supplier Material materials with Water absorption of 1.7 % | @24 hours | ASTM D570 |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongation | 23.0 °C | 13 % Show Supplier Material materials with Elongation of 13 % | ASTM D638 | ||
Flexural modulus | 23.0 °C | 1.8 GPa Show Supplier Material materials with Flexural modulus of 1.8 GPa | ASTM D790 | ||
Flexural strength | 23.0 °C | 55 MPa Show Supplier Material materials with Flexural strength of 55 MPa | ASTM D790 | ||
Hardness, Rockwell R | 23.0 °C | 105 [-] Show Supplier Material materials with Hardness, Rockwell R of 105 [-] | ASTM D785 | ||
Hardness, Shore D | 23.0 °C | 68 [-] Show Supplier Material materials with Hardness, Shore D of 68 [-] | ASTM D2240 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 320 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 320 J/m | ASTM D256 | ||
Yield strength | 23.0 °C | 34 MPa Show Supplier Material materials with Yield strength of 34 MPa | ASTM D638 | ||
Impact strength, Izod unnotched, ASTM | No Break, ASTM D256 |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 88 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 88 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 71 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 71 °C | ASTM D648 | |
Flammability | UL94: BH |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+9 - 1.00E+11 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+9 - 1.00E+11 Ω/sq | ASTM D257 |
Volume resistivity | 23.0 °C | 1.00E+9 - 1.00E+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+9 - 1.00E+11 Ω·cm | ASTM D257 |
Technological properties
Property | ||
---|---|---|
Application areas |