General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.28 g/cm³ Show Material materials with Density of 7.28 g/cm³ | Typical for Pure/Low Alloyed Tin |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.1E-5 - 2.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.1E-5 - 2.9E-5 1/K | Typical for Pure/Low Alloyed Tin |
Melting point | 232 °C Show Material materials with Melting point of 232 °C | Typical for Pure/Low Alloyed Tin | |
Specific heat capacity | 23.0 °C | 205 - 238 J/(kg·K) Show Material materials with Specific heat capacity of 205 - 238 J/(kg·K) | Typical for Pure/Low Alloyed Tin |
Thermal conductivity | 23.0 °C | 52 - 74 W/(m·K) Show Material materials with Thermal conductivity of 52 - 74 W/(m·K) | Typical for Pure/Low Alloyed Tin |
Chemical properties
Property | Value |
---|---|
Tin | 99 % Show Material materials with Tin of 99 % |