Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 215 - 350 °C Show Material materials with Melting point of 215 - 350 °C | Typical for Tin Antimony | |
Thermal conductivity | 23.0 °C | 40 W/(m·K) Show Material materials with Thermal conductivity of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Antimony | 4.5 - 8 % Show Material materials with Antimony of 4.5 - 8 % |
Bismuth | 0.5 % Show Material materials with Bismuth of 0.5 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Copper | 0.25 - 2 % Show Material materials with Copper of 0.25 - 2 % |
Lead | 0.25 % Show Material materials with Lead of 0.25 % |
Silver | 0.05 % Show Material materials with Silver of 0.05 % |
Tin | 91.5 % Show Material materials with Tin of 91.5 % |