Mechanical
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 215 - 350 °C Show Material materials with Melting point of 215 - 350 °C | Typical for Tin Antimony | |
Thermal conductivity | 23.0 °C | 40 W/(m·K) Show Material materials with Thermal conductivity of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 12 - 14 % Show Material materials with Antimony of 12 - 14 % |
Arsenic | 0.08 % Show Material materials with Arsenic of 0.08 % |
Copper | 2 - 3 % Show Material materials with Copper of 2 - 3 % |
Iron | 0.08 % Show Material materials with Iron of 0.08 % |
Tin | 59 - 61 % Show Material materials with Tin of 59 - 61 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |