ASTM B352 Grade R60901 soft annealed (+A)

Want to keep this datasheet? Save it now in your required format

Description

Highly corrosion-resistant zirconium-niobium sheet, strip and plate for nuclear application.

Related Standards

Properties

General

Density

ρ

6.55 g/cm³ at 20 °C

Mechanical

Elongation A50

A50

20 % at 20 °C

Show Zirconium materials with Elongation A50 of 20 % at 20 °C

Elongation A50, transverse

A50,trans

20 % at 20 °C

Show Zirconium materials with Elongation A50, transverse of 20 % at 20 °C

Tensile strength

Rm

450 MPa at 20 °C

Show Zirconium materials with Tensile strength of 450 MPa at 20 °C

Tensile strength, transverse

Rm,trans

450 MPa at 20 °C

Show Zirconium materials with Tensile strength, transverse of 450 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

310 MPa at 20 °C

Show Zirconium materials with Yield strength Rp0.2 of 310 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

345 MPa at 20 °C

Show Zirconium materials with Yield strength Rp0.2, transverse of 345 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Nb

2.4 - 2.8 %

O

0.09 - 0.15 %

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.