Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Carbon | 0.025 % Show Material materials with Carbon of 0.025 % |
Chromium | 0.05 % Show Material materials with Chromium of 0.05 % |
Hydrogen | 5E-3 % Show Material materials with Hydrogen of 5E-3 % |
Iron | 0.08 % Show Material materials with Iron of 0.08 % |
Nitrogen | 0.02 % Show Material materials with Nitrogen of 0.02 % |
Oxygen | 0.13 % Show Material materials with Oxygen of 0.13 % |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % |