Hafnium strip, sheet and plate for alloying.

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Carbon

0.025 %

Show Material materials with Carbon of 0.025 %

Chromium

0.05 %

Show Material materials with Chromium of 0.05 %

Hydrogen

5E-3 %

Show Material materials with Hydrogen of 5E-3 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Nitrogen

0.02 %

Show Material materials with Nitrogen of 0.02 %

Oxygen

0.13 %

Show Material materials with Oxygen of 0.13 %

Silicon

0.05 %

Show Material materials with Silicon of 0.05 %

Titanium

0.05 %

Show Material materials with Titanium of 0.05 %

Tungsten

0.02 %