General
Property | Value | Comment |
---|---|---|
Density | 4.506 g/cm³ Show Material materials with Density of 4.506 g/cm³ | Typical for Titanium |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 120.0 GPa Show Material materials with Elastic modulus of 120.0 GPa | Typical for Titanium | |||
Elongation | 20.0 °C | 15.0 % Show Material materials with Elongation of 15.0 % | As-Cast | DIN 17865 | |
Tensile strength | 20.0 °C | 350.0 MPa Show Material materials with Tensile strength of 350.0 MPa | As-Cast | DIN 17865 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |||
Melting point | 1668.0 °C Show Material materials with Melting point of 1668.0 °C | Typical for Titanium | |||
Thermal conductivity | 20.0 °C | 16.3 W/(m·K) Show Material materials with Thermal conductivity of 16.3 W/(m·K) | As-Cast | DIN 17865 |
Electrical
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Electrical conductivity | 20.0 °C | 1750000.0 S/m Show Material materials with Electrical conductivity of 1750000.0 S/m | As-Cast | DIN 17865 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Carbon | 0.1 Show Material materials with Carbon of 0.1 | As-Cast | DIN 17865 |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | As-Cast | DIN 17865 |
Iron | 0.2 Show Material materials with Iron of 0.2 | As-Cast | DIN 17865 |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | As-Cast | DIN 17865 |
Oxygen | 0.4 Show Material materials with Oxygen of 0.4 | As-Cast | DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, compact casting, separately cast test samples or taken from casting without ingate |