DIN 17865 Grade G-Ti3 As-Cast

Want to keep this datasheet? Save it now in your required format

Description

Castings made from G-Ti3 with the material number 3.7051 are preferably applied in the apparatus construction as well as for application purposes with demands on the corrosion-resistance, e.g. in the chemical industry, paper, cellulose, textile and food industry, in the energy extraction and maritime technology, in the galvanic technology and the surface refinement as well as in the medical technology. In reducing mediums, the corrosion-resistance is worse than with the palladium-alloyed material G-Ti3Pd.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

4.506 g/cm³

Show Material materials with Density of 4.506 g/cm³

Typical for Titanium

Mechanical

PropertyTemperatureValueConditionRelated StandardsComment

Elastic modulus

100.0 - 120.0 GPa

Show Material materials with Elastic modulus of 100.0 - 120.0 GPa

Typical for Titanium Near Alpha Alloy

Elongation

20.0 °C

12.0 %

Show Material materials with Elongation of 12.0 %

As-Cast

DIN 17865

Tensile strength

20.0 °C

450.0 MPa

Show Material materials with Tensile strength of 450.0 MPa

As-Cast

DIN 17865

Thermal

PropertyTemperatureValueConditionRelated StandardsComment

Coefficient of thermal expansion

7.599999999999997e-06 - 1.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 1.1e-05 1/K

Typical for Titanium Near Alpha Alloy

Melting point

1540.0 - 1715.0 °C

Show Material materials with Melting point of 1540.0 - 1715.0 °C

Typical for Titanium Near Alpha Alloy

Specific heat capacity

460.0 - 527.0 J/(kg·K)

Show Material materials with Specific heat capacity of 460.0 - 527.0 J/(kg·K)

Typical for Titanium Near Alpha Alloy

Thermal conductivity

20.0 °C

16.3 W/(m·K)

Show Material materials with Thermal conductivity of 16.3 W/(m·K)

As-Cast

DIN 17865

Electrical

PropertyTemperatureValueConditionRelated Standards

Electrical conductivity

20.0 °C

1750000.0 S/m

Show Material materials with Electrical conductivity of 1750000.0 S/m

As-Cast

DIN 17865

Chemical properties

PropertyValueConditionRelated Standards

Carbon

0.1

Show Material materials with Carbon of 0.1

As-Cast

DIN 17865

Hydrogen

0.015

Show Material materials with Hydrogen of 0.015

As-Cast

DIN 17865

Iron

0.25

Show Material materials with Iron of 0.25

As-Cast

DIN 17865

Nitrogen

0.05

Show Material materials with Nitrogen of 0.05

As-Cast

DIN 17865

Oxygen

0.4

Show Material materials with Oxygen of 0.4

As-Cast

DIN 17865

Technological properties

Property
Processing methods

investment casting, compact casting, separately cast test samples or taken from casting without ingate