General
Property | Value | Comment |
---|---|---|
Density | 4.506 g/cm³ Show Material materials with Density of 4.506 g/cm³ | Typical for Titanium |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 120.0 GPa Show Material materials with Elastic modulus of 120.0 GPa | Typical for Titanium | |||
Elongation | 20.0 °C | 5.0 % Show Material materials with Elongation of 5.0 % | As-Cast | DIN 17865 | |
Tensile strength | 20.0 °C | 900.0 MPa Show Material materials with Tensile strength of 900.0 MPa | As-Cast | DIN 17865 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium |
Melting point | 1668.0 °C Show Material materials with Melting point of 1668.0 °C | Typical for Titanium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 5.7 - 6.3 % Show Material materials with Aluminium of 5.7 - 6.3 % | As-Cast | DIN 17865 |
Carbon | 0.1 Show Material materials with Carbon of 0.1 | As-Cast | DIN 17865 |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | As-Cast | DIN 17865 |
Iron | 0.2 Show Material materials with Iron of 0.2 | As-Cast | DIN 17865 |
Molybdenum | 0.25 - 0.75 % Show Material materials with Molybdenum of 0.25 - 0.75 % | As-Cast | DIN 17865 |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | As-Cast | DIN 17865 |
Oxygen | 0.3 Show Material materials with Oxygen of 0.3 | As-Cast | DIN 17865 |
Silicon | 0.1 - 0.4 % Show Material materials with Silicon of 0.1 - 0.4 % | As-Cast | DIN 17865 |
Zirconium | 4.0 - 6.0 % Show Material materials with Zirconium of 4.0 - 6.0 % | As-Cast | DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, compact casting, separately cast test samples or taken from casting without ingate |