General
Property | Value | Comment |
---|---|---|
Density | 4.506 g/cm³ Show Material materials with Density of 4.506 g/cm³ | Typical for Titanium |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elastic modulus | 120.0 GPa Show Material materials with Elastic modulus of 120.0 GPa | Typical for Titanium | |||
Elongation | 20.0 °C | 5.0 % Show Material materials with Elongation of 5.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Reduction of area | 20.0 °C | 10.0 % Show Material materials with Reduction of area of 10.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Tensile strength | 20.0 °C | 880.0 MPa Show Material materials with Tensile strength of 880.0 MPa | Annealed | WL 3.7264-1, DIN 17865 |
Thermal
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |||
Melting point | 1668.0 °C Show Material materials with Melting point of 1668.0 °C | Typical for Titanium | |||
Thermal conductivity | 20.0 °C | 7.1 W/(m·K) Show Material materials with Thermal conductivity of 7.1 W/(m·K) | Annealed | WL 3.7264-1, DIN 17865 |
Electrical
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Electrical conductivity | 20.0 °C | 580000.0 S/m Show Material materials with Electrical conductivity of 580000.0 S/m | Annealed | WL 3.7264-1, DIN 17865 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminium | 5.5 - 6.7 % Show Material materials with Aluminium of 5.5 - 6.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Carbon | 0.1 Show Material materials with Carbon of 0.1 | Annealed | WL 3.7264-1, DIN 17865 |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | Annealed | WL 3.7264-1, DIN 17865 |
Iron | 0.3 Show Material materials with Iron of 0.3 | Annealed | WL 3.7264-1, DIN 17865 |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Annealed | WL 3.7264-1, DIN 17865 |
Oxygen | 0.25 Show Material materials with Oxygen of 0.25 | Annealed | WL 3.7264-1, DIN 17865 |
Titanium | 87.7 % Show Material materials with Titanium of 87.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Vanadium | 3.5 - 4.5 % Show Material materials with Vanadium of 3.5 - 4.5 % | Annealed | WL 3.7264-1, DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, sample taken from casting or separately cast or cast on |