General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 5.3 g/cm³ Show Material materials with Density of 5.3 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Zinc Aluminium |
Tensile strength | 20.0 °C | 230 - 290 MPa Show Material materials with Tensile strength of 230 - 290 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Melting point | 375 - 485 °C Show Material materials with Melting point of 375 - 485 °C | Typical for Zinc Aluminium | |
Specific heat capacity | 20.0 °C | 502 J/(kg·K) Show Material materials with Specific heat capacity of 502 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 130 W/(m·K) Show Material materials with Thermal conductivity of 130 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 2.00E+7 S/m Show Material materials with Electrical conductivity of 2.00E+7 S/m |