General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.13 g/cm³ Show Material materials with Density of 7.13 g/cm³ | Typical for Zinc |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 105 GPa Show Material materials with Elastic modulus of 105 GPa | Typical for Zinc |
Elongation A10 | 20.0 °C | 30 - 50 % Show Material materials with Elongation A10 of 30 - 50 % | |
Hardness, Brinell | 20.0 °C | 60 - 80 [-] Show Material materials with Hardness, Brinell of 60 - 80 [-] | |
Poisson's ratio | 23.0 °C | 0.25 [-] Show Material materials with Poisson's ratio of 0.25 [-] | Typical for Zinc |
Shear modulus | 23.0 °C | 42 GPa Show Material materials with Shear modulus of 42 GPa | Typical for Zinc |
Tensile strength | 20.0 °C | 250 - 300 MPa Show Material materials with Tensile strength of 250 - 300 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Melting point | 380 - 420 °C Show Material materials with Melting point of 380 - 420 °C | Typical for Zinc | |
Specific heat capacity | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 272 - 525 J/(kg·K) | Typical for Zinc |
Thermal conductivity | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Thermal conductivity of 105 - 125 W/(m·K) | Typical for Zinc |